simbol slivostiAWS A5.16/A5.16M: 2013Klasifikacija svemirskih materijalaJIS Z3331:2011DIN 1737-1: 1984
digitalni markeroznaka hemijskog simbola
Ti 0100Ti99.8ERTI-1-STi 01003.702 6
Ti 0120Ti99.6ERTI-2-STi 0120-
Ti 0125Ti99.5ERTI-3AMS 4951:2003STi 0125-
Ti 0130Ti99.3ERTI-4-STi 01303.703 6
Ti 2251TiPd0.2ERTI-11-STi 22513,7226
Ti 2253TiPd0.6ERTI-17-STi 2253-
Ti 2255TiRu0.1ERTI-27-STi 2255-
Ti 2401TiPd0.2AERTI-7-STi 24013,723 6
Ti 2403TiPd0.6AERTI-16-STi 2403-
Ti 2405TiRu0.1AERTI-26-STi 2405-
Ti 3401TiNi0.7Mo0.3ERTI-12-STi 3401-
Ti 3416TiRu0.05Ni0.05ERTI-15A-STi 3416-
Ti 3423TiNi0.5ERTI-13-STi 3423-
Ti 3424TiNi0.5AERTI-14-STi 3424-
Ti 3443TiNi0.45Cr0.15ERTI-33-STi 3443-
Ti 3444TiNi0.45Cr0.15AERTI-34-STi 3444-
Ti 3531TiCo0.5ERTI-30-STi 3531-
Ti 3533TiCo9.5AERTI-31-STi 3533-
Ti 4251TiAl4V2ERTI-38---
Ti 4621TiAl6Zr4Mo2Sn2-AMS 4952:2007STi 4621-
Ti 4810TiA18V1Mo-AMS 4955:2008STi 4810--
Ti 5112TiA15V1SnMo1ZrlERTI-32-STi 5112-
Ti 6321TiAI3V2.5AERTI-9-STi 6321-
Ti 6324TiAl3V2.5RuERTI-28-STi 6324-
Ti 6326TiAl3V2.5PdERTI-18-STi 6326-
Ti 6402TiAl6V4BERTI-5AMS 4954:2003STi 6402-
Ti 6408TiAl6V4AERTI-23AMS 4956:2003ST:6408-
Ti 6413TiAl6V4Ni0.5PdERTI-25-STi 6413-